It is used for element addition of nonferrous metal alloys. It melts fast when putting into the melt under perature ( usually less than 5 minutes,in which fast melting of silicon is usually less than 10 minutes.It is simple for use and the recovery rate of element in additive is more than 90%.)
|
|
|
|
| Packing︰ | 2kg/bag;20kg/ctn |
| Standards Certificate︰ | ISO9001 |
| specifications︰ | 40% 60% 70% 75% 80% 85%Ti |
| Export Markets︰ | China |
| Payment Details︰ | c&c |
| Min Order︰ | 500kgs |
| Standard Met︰ | iso9001 |
|
|
|